Temperature-dependent voltage degradation and LeTID kinetics in n-type interdigitated back contact (IBC) solar cells

  • Yousuf, Hasnain; 
  • Alamgeer,; 
  • Rahman, Rafi ur; 
  • Mungmung, Chu; 
  • Aida, Maha Nur; 
  • ... Yi, Junsin; 
  • 외 4명
Citations

WEB OF SCIENCE

1
Citations

SCOPUS

1

초록

This work systematically investigates temperature-dependent performance and light- and elevated-temperature-induced degradation (LeTID) in an n-type crystalline silicon interdigitated back contact (IBC) solar cell. Illuminated current–voltage characteristics were measured from 25 to 85 °C under AM1.5G 1-sun conditions (100 mW cm−2), combined with time-resolved LeTID stress (up to 960 min) and temperature-dependent dark I – V analysis. At 25 °C, the device exhibited Jsc ≈ 38.6 mA cm−2, Voc ≈ 0.743 V, FF ≈ 79%, and η ≈ 22.7%. Increasing temperature to 85 °C produced a modest ∼ 3% rise in Jsc (+0.0203 mA cm−2 K−1, ∼+0.05% K−1), while Voc decreased linearly with a coefficient of − 1.4 mV K−1 (≈ −0.2% K−1), leading to an overall efficiency reduction of ∼ 9%. The fill factor showed minimal temperature dependence, confirming that thermal losses are predominantly voltage-driven. Under continuous one-sun LeTID stress at 45–85 °C, degradation kinetics were strongly temperature-accelerated. At 85 °C, Voc exhibited rapid early-time decay within 10–30 min before stabilizing, whereas Jsc remained within ± 2% (relative variation). Dark I – V analysis revealed exponential growth of the dark saturation current density ( J0 ) and pronounced reduction in shunt resistance with temperature. Arrhenius analysis of shunt conductance yielded an activation energy of ∼ 1.10 eV, indicating thermally activated leakage behavior. A defect-augmented recombination framework linking temperature-dependent defect density to J0 ( t , T ) consistently explains illuminated voltage degradation, LeTID kinetics, and dark leakage evolution. Extrapolation to typical operating temperatures (∼60 °C) predicts ∼ 49 mV voltage loss relative to standard test conditions, underscoring voltage stability as a key reliability factor for high-efficiency rear-contact photovoltaic devices in warm climates.

키워드

Arrhenius activation energy; Crystalline silicon n-type; DarkI–V analysis; IBC solar cell; LeTID; Recombination; Temperature effects; CARRIER-INDUCED DEGRADATION; ELEVATED-TEMPERATURE; SILICON; PASSIVATION; PERFORMANCE
제목
Temperature-dependent voltage degradation and LeTID kinetics in n-type interdigitated back contact (IBC) solar cells
저자
Yousuf, Hasnain; Alamgeer,; Rahman, Rafi ur; Mungmung, Chu; Aida, Maha Nur; Mohammed, Shurouq Abdulqadir; Wang, Xiaobo; Jin, Hyejeong; Khokhar, Muhammad Quddamah; Yi, Junsin
DOI
10.1016/j.solener.2026.114738
발행일
2026-09-01
유형
Article
저널명
Solar Energy
권
315